      Generally a crack of cold joint will be chipped out using a concrete chisel bit to 1" (25mm) wide by 1.5" (37mm) deep.  The slot will then be coated with Xypex Concentrate in slurry form and then filled with either Xypex Concentrate in dry pack or a combination of Xypex Patch'n' Plug and Xypex Concentrate in dry pack.  Note that many waterproofing repair professionals will have variations on this procedure that are acceptable.
      Posted on 26 Nov 2012

This site contains user submitted content, comments and opinions and is for informational purposes only. Xypex disclaims any and all liability for the acts, omissions and conduct of any third parties in connection with or related to your use of the site. All postings and use of the content on this site are subject to the Xypex Support Communities Terms of Use.